UV LED wood coating curing

Summary: UV LED curing uses a wavelength (commonly 395 nm) to start photopolymerisation; dose = irradiance x time. LED power, distance and line speed must match film thickness and pigment absorption, else surface-dry/soft-inside or over-cure.

Mechanism

Dark/pigmented films absorb/shield UV and need more energy or multi-lamp/double-side; too little energy gives low crosslink density and poor chemical resistance.

Key data

  • Typical UVA-LED 395 nm must match the photoinitiator's absorption.
  • Dose is in mJ/cm2; both under- and over-dose hurt performance.
  • Higher line speed needs more power or longer exposure to hold dose.

Matching

VariableResult
Under-doseSkin-cure, soft inside, poor chemical
Over-doseYellowing, brittleness, energy waste

Defects & fixes

  • Soft inside: low energy / big distance — raise dose.
  • Deep tackiness: pigment shielding — multi-lamp/double-side or thinner.
  • Yellow/brittle: over-exposure — match power/speed.

FAQ

Why LED over mercury?

Cold cure, low energy, no ozone, instant on/off, good for thin wood parts.

Why is dark hard to cure?

Pigments absorb/shield UV; need higher dose or angled exposure.

How to set energy?

Small-sample by thickness, colour, initiator and line speed to find the window that hits hardness and chemical.